Note: Ingredients listed on restricted chemical lists
EC/CAS
200-659-6/67-56-1
Name of the chemical
Methanol
Concentration
<1
EC/CAS
200-831-0/75-01-4
Name of the chemical
Chloroethylene
Concentration
<0.005%
General Information
Revision date
2015-05-01
Product name
SOLBIN TA3
Chemical name
Vinyl Resin
1.2.1 Relevant identified uses
This product is intended for use as an additive for coatings, inks, paints, and adhesives
supplier name
Shin-Etsu MicroSi, Inc
Manufacturer Name
Nissin Chemical Industry Co., Ltd
Emergency telephone
(800) 424-9300
Icons in SDS
Company Information
company name
Nissin Chemical Industry Co., Ltd
e-mail address of the competent person responsible for the Safety Data Sheet
csteam@microsi.com
GHS Information
Signal word
Warning
Hazard Codes
Hazard statements (CLP)
H371
Hazard statements
Code
Statements
H371
May cause damage to organs
Section 2
SECTION 2: Hazards identification
Hazard categories
Specific Target Organ Toxicity – Single Exposure Category 2 Combustible Dust
Signal word
Warning
Hazard statements
H371 May cause damage to organs
Prevention
P260 Do not breathe dust/fuel/gas/mist/vapors/spray. P264 Wash hands thoroughly after handling P270 Do not eat, drink, or smoke when using this product.
Response
P308 + P311 IF exposed or concerned: Call a POISON Center or doctor.
Storage
P405 Store locked up.
Disposal
P501 Dispose of contents/container: Follow the waste disposal requirements of your country, state, or local authorities. <97 % of mixture consists of ingredients of unknown acute toxicity
2.3 Other hazards
None
2.1 Classification of the substance or mixture
FIRE AND EXPLOSION Not Hazardous May form flammable / explosive dust-air mixture. APPEARANCE White fine powder
NFPA Ratings
Component Health Flammability Instability Special (Blue) (Red) (Yellow) (White) SOLBIN TA3 1 0 0 -- SAFETY NOTICE—VINYL CHLORIDE EXPOSURE The manufacturing process of Solbin products results in residual Vinyl Chloride (VC) being contained in the product. During shipment, the exposure of this product to ambient temperatures causes the residual VC to volatilize and accumulate within the shipping container. Vinyl Chloride has both a very low flash point (-108 °F) and boiling point (7 °F). Ambient air testing has been conducted to determine the initial concentration of VC that an employee may be exposed to when opening the container doors prior to unloading the product.